MOQ: | 100KGS |
Price: | 2.15 USD/KG |
Standard Packaging: | Wooden Pallet |
Delivery Period: | 7 Days |
Payment Method: | L/C, T/T |
Supply Capacity: | 50000KGS |
Stainless Steel 439, UNS S43035, SS439, SUS439, 1.4510
SS439 is an 18% chromium, titanium stabilized ferritic stainless steel with corrosion resistance similar to that of 304/304L stainless steel. This grade may be used in the annealed, cold formed or as-welded condition in applications where other stainless steels such as Type 304/304L and Type 430 are used. Type 439 has good weldability due to titanium stabilization and has excellent resistance to stress corrosion cracking. Type 439 outperforms Type 409 in both oxidation and corrosion resistance and typical applications include tubular manifolds and exhaust system components. where temperatures tend to go beyond the oxidation limit of grade 409 steel. It is also preferred where wet corrosion resistance especially to chlorides is needed.
439 stainless steel Chemical Composition
Chemical Composition (wt%) limits as specified in ASTM A240 and ASME SA240*
Element | 439 |
Carbon | 0.030 |
Chromium | 17.0-19.0 |
Nickel | 0.50 |
Manganese | 1.00 |
Silicon | 1.00 |
Nitrogen | 0.030 |
Phosphorus | 0.040 |
Sulfur | 0.030 |
Aluminum | 0.15 |
Titanium | 0.20 +4(C+N) min 1.10 max |
* Maximum, unless range is indicated
Stainless steel grade 439 Mechanical Properties
Mechanical property requirements for annealed product as specified in ASTM A240 and ASME SA240
Property | 439 |
Yield Strength, min. (ksi) | 30 |
Tensile Strength, min. (ksi) | 60 |
Elongation, min. (%) | 22 |
Hardness, max. (Rb) | 89 |
Physical properties for grade 439 stainless steel
Property | 439 |
Density, lb/in3 | 0.278 |
Modulus of Elasticity, psi | 29.0 x 106 |
Coefficient of Thermal Expansion, 68-212˚F, /˚F | 5.6 x 10-6 |
Thermal Conductivity, Btu/ft hr ˚F | 14.0 |
Specific Heat, Btu/lb ˚F | 0.11 |
Electrical Resistivity, Microohm-in | 24.8 |
Data are typical, are provided for informational purposes, and should not be construed as maximum or minimum values for specification or for final design, or for a particular use or application. The data may be revised anytime without notice.
MOQ: | 100KGS |
Price: | 2.15 USD/KG |
Standard Packaging: | Wooden Pallet |
Delivery Period: | 7 Days |
Payment Method: | L/C, T/T |
Supply Capacity: | 50000KGS |
Stainless Steel 439, UNS S43035, SS439, SUS439, 1.4510
SS439 is an 18% chromium, titanium stabilized ferritic stainless steel with corrosion resistance similar to that of 304/304L stainless steel. This grade may be used in the annealed, cold formed or as-welded condition in applications where other stainless steels such as Type 304/304L and Type 430 are used. Type 439 has good weldability due to titanium stabilization and has excellent resistance to stress corrosion cracking. Type 439 outperforms Type 409 in both oxidation and corrosion resistance and typical applications include tubular manifolds and exhaust system components. where temperatures tend to go beyond the oxidation limit of grade 409 steel. It is also preferred where wet corrosion resistance especially to chlorides is needed.
439 stainless steel Chemical Composition
Chemical Composition (wt%) limits as specified in ASTM A240 and ASME SA240*
Element | 439 |
Carbon | 0.030 |
Chromium | 17.0-19.0 |
Nickel | 0.50 |
Manganese | 1.00 |
Silicon | 1.00 |
Nitrogen | 0.030 |
Phosphorus | 0.040 |
Sulfur | 0.030 |
Aluminum | 0.15 |
Titanium | 0.20 +4(C+N) min 1.10 max |
* Maximum, unless range is indicated
Stainless steel grade 439 Mechanical Properties
Mechanical property requirements for annealed product as specified in ASTM A240 and ASME SA240
Property | 439 |
Yield Strength, min. (ksi) | 30 |
Tensile Strength, min. (ksi) | 60 |
Elongation, min. (%) | 22 |
Hardness, max. (Rb) | 89 |
Physical properties for grade 439 stainless steel
Property | 439 |
Density, lb/in3 | 0.278 |
Modulus of Elasticity, psi | 29.0 x 106 |
Coefficient of Thermal Expansion, 68-212˚F, /˚F | 5.6 x 10-6 |
Thermal Conductivity, Btu/ft hr ˚F | 14.0 |
Specific Heat, Btu/lb ˚F | 0.11 |
Electrical Resistivity, Microohm-in | 24.8 |
Data are typical, are provided for informational purposes, and should not be construed as maximum or minimum values for specification or for final design, or for a particular use or application. The data may be revised anytime without notice.